Acid Protection Textile Industry; multiple uses, concrete and metal,acid protection

We are pleased to inform you that we have applied your product “SEAL-IT 429 S.T.U.F.” at the following units of our factory with utmost success. Thanks to “SEAL-IT 429 S.T.U.F.”, the need to use stainless steel in corrosive environments has been eliminated to a great extent. Besides, protective effect of “SEAL-IT 429 S.T.U.F.” on building floors and walls that are exposed to acids and similar corrosive chemicals has significantly helped to reduce construction maintenance and repair costs.

Fields of application:

Dye-House Floor: “SEAL-IT 429 S.T.U.F.” coating which was initially applied at a certain part of the dye- house floor has not shown any sign of damage for longer than a year. Subject coating has been successfully protecting the concrete floor from the effects of acidic environment (65% acetic acid).

Upon this successful result, all floors in dye preparation and print application section of newly established sample carpet print unit have been covered with “SEAL-IT 429 S.T.U.F.”.

Mixing Unit Pipelines: These pipes and flap valves (through which moist fibres pass) have been applied “SEAL-IT 429 S.T.U.F.”. After application of the product, problems due to moisture have been eliminated. Success of the coating is being continuously observed for the last 9 months.

Covering Unit Cylinders: Cylinders whose paint coats were previously swelling and cracking in a short time due to exposure to the effects of dense vapour have been applied “SEAL-IT 429 S.T.U.F.”. although a periods of 4 months has passed after application of the product, still there are no signs of damage, wear, swelling or cracking on the paint coats.

Waste Water Treatment Plant: In this plant, all metallic components which are in direct contact with waste water have been coated with “SEAL-IT 429 S.T.U.F.”. A thick layer of rust has formed on certain metal surfaces which were left uncoated for test purposes whereas coated surfaces still keep their original appearance.